Paddock Mat SD "Anthracite"
- /
-
Ready to ship
from stock in 1-3 days - €56.20 / 2 Piece / m²
- (14.00 kg / Piece)
EAN: 4251469366466 | Item no.: 6646
The Paddock Mat is made from rubber granules bonded with polyurethane. It is intended for paddocks, stables, loose housing and field shelters. The mats let rainwater pass through and are frost-resistant. They have a slip-resistant surface and give slightly under the hoof.
How do paddock mats help horses?
Horses need a dry place to stand. If they stand on wet ground for long periods, the hoof horn softens. This can lead to thrush and mud fever. In autumn and winter, some paddocks become muddy. Areas in front of the field shelter and around the hay feeder are often particularly muddy. Paddock mats let rainwater pass through. If they are laid on a base that allows the water to drain away, hardly any puddles form. Horses then have a dry surface to stand on even after days of rain. Paddock mats are slip-resistant both when dry and when wet. This helps a horse lie down and get back up in a stable or field shelter.
How are paddock tiles laid?
The base must be load-bearing, level and water-permeable. Gravel grids filled with chippings are well suited. Lay the paddock tiles on top without adhesive in a random bond pattern, so the joints are staggered. The area needs a firm edge restraint on all sides. This prevents the tiles from moving apart.
Do paddock mats need bedding?
Horses do not like urinating on a firm surface because it splashes. They are also reluctant to urinate on paddock mats. For this reason, straw or shavings are used as bedding in stables, loose housing and field shelters, or a separate toilet area is provided. In the paddock, horses need an unsurfaced area where they can urinate.
What are paddock mats made from?
Paddock mats are made from coarse rubber granules from old car tyres. A polyurethane binder holds the granules together. Small gaps remain between the granules. Water drains through these gaps. The rubber mats are frost-resistant. Frost does not damage them even when they are wet. They are not designed to be driven over regularly by a yard loader or tractor.
Discount
Product Highlights
Characteristics
Product Details – Material and Structure
Comparative values
Rubber tiles and rubber mats from WARCO are not harmful to health when used as intended. They are made from rubber granules bound with PU; the solvent-free PU binder cures fully during manufacture.
The rubber granules are predominantly recycled from end-of-life tyres (ELTs). The PAH content of ELT rubber granules may vary according to origin and batch; PAH means polycyclic aromatic hydrocarbons. Black ELT rubber granules contain carbon black, a fine industrial soot that gives the rubber its black colour. Surface abrasion may occur during use of rubber mats.
In two-layer versions, the wearing layer is made from newly manufactured EPDM, which is coloured throughout and free from harmful substances. The possible PAH variations associated with ELT rubber granules do not occur with EPDM. Versions with an EPDM wearing layer are particularly suitable for prolonged or intensive skin contact and for areas intended for babies. The relevant product description states whether a product has a two-layer construction.
WARCO rubber tiles are made from rubber granules bound with polyurethane. Each granule is coated with polyurethane and held within the binder. The solvent-free binder cures fully during manufacture. Individual granules may remain attached to a tile after manufacture or come loose while the tiles are being laid. Any such manufacturing residue can be swept up or removed with a vacuum cleaner.
Vulcanised rubber and cured polyurethane are insoluble in water. Rainwater passing through the porous tiles does not dissolve these constituents. The same applies to individual granules left on the surface. On this basis, contamination of the soil or groundwater is not expected.
Rubber tiles and rubber mats made from PU-bound rubber granules typically have a service life of around 10 to 15 years, although this can vary substantially with the conditions of use. Some surfaces remain in use for more than 20 years, while others require replacement after only a few years.
The type and intensity of loading determine service life. Friction causes surface wear, while high or sustained compressive loads can affect the material structure. Mechanical loading is generally lower in private settings than in commercial use. Weathering also affects service life, particularly UV radiation, temperature changes and frequent freeze-thaw cycles.
The type of granules influences ageing behaviour. An EPDM wearing layer is UV-resistant and, after an initial acclimatisation period, remains largely colour-stable. ELT granules with a pigmented binder become darker over time.
The data sheet for each WARCO product provides information on UV resistance, colour fastness and abrasion resistance, helping to select the appropriate covering. Correct installation in accordance with the installation guidelines on a level, load-bearing substrate also contributes to a long service life.
Outdoor rubber tiles made from polyurethane-bound rubber granules are frost-resistant and suitable for use throughout the winter. Their porous structure absorbs precipitation and allows it to pass downwards; water remaining in the pores has space to expand when it freezes, while the rubber granules and polyurethane binder remain elastic at sub-zero temperatures. The sub-base must also be constructed to withstand frost.
On bound sub-bases, water flows beneath and between the tiles in the direction of the fall towards the drainage system. On chippings or crushed stone, it drains vertically through the construction. If water collects beneath the tiles, a frost-susceptible sub-base may rise and then settle again after thawing. The tiles themselves remain unaffected, but the surface may become more uneven.
For winter maintenance, use a snow shovel with a smooth edge and avoid catching the tile edges. Salt used in normal quantities to melt ice does not harm the rubber granules.
Rubber tiles can be water-permeable at rates ranging from nearly zero to more than 1,100 litres per square metre per hour. Water permeability depends on the particle-size fraction of the rubber granules used and on the pressing pressure applied during manufacture. The tiles are made from PU-bound rubber granules and have an open-pored structure.
Within this porous structure, water does not pass through the rubber itself but through the voids between the bonded granules. The more tightly the granules are compacted, the less water a rubber tile allows through. At low pressing pressure, the irregularly shaped granules sit loosely beside one another, leaving interconnected pores and fine channels through which water flows vertically downwards. An accredited institute measured more than 1,100 litres per square metre per hour in accordance with BS EN 12616, even after four weeks of weathering.
The respective water permeability value is stated as a comparative value in the product description. Rubber tiles made under high pressing pressure have an almost void-free granule structure and allow hardly any water through. A newly laid area absorbs water more slowly during its first days than the measured value may suggest, because the granule surfaces initially resist wetting, much like a new rain jacket. After several days of use, the floor covering reaches its full water permeability; scrubbing it with a little washing-up liquid speeds up this process.
The test report can be submitted to building authorities as evidence of water permeability. How an area is classified depends on the overall system build-up: precipitation can drain through the floor covering into the ground only if the sub-base beneath the rubber tiles also absorbs water.
Thermal insulation from floor coverings made from rubber granules is supplementary and varies with the product design and thickness; it does not replace the thermal insulation required within the building structure. Across the WARCO range, thermal conductivity is approximately 0.07 to 0.16 W/(m·K), depending on the product line. By comparison, EPS insulation materials achieve approximately 0.032 to 0.040 W/(m·K), so they provide substantially greater insulation than floor coverings made from rubber granules at the same thickness.
Thermal conductivity and thickness determine the thermal resistance of a floor covering: lower thermal conductivity produces greater thermal resistance, as does a thicker covering. On a cool mineral substrate, a dry covering made from rubber granules draws heat from the foot more slowly and therefore feels less cold. With porous outdoor coverings, thermal insulation decreases when wet because water conducts heat more readily than the air within the pores.
For the thermal insulation of flat roofs and ceilings, the performance of the complete roof or ceiling build-up is decisive. With underfloor heating, the thermal resistance of the covering slows heat output into the room; the thicker the floor covering, the greater this slowing effect.
Rubber granule mats of any thickness can be cut with a jigsaw or a circular saw. A circular saw is suited to straight cuts, while a jigsaw is suited to curved cuts and cut-outs. PU-bound rubber granules can be worked in much the same way as wood, provided both saws are guided steadily with an even feed rate.
For particularly thick rubber mats or large sections to be cut, a reciprocating saw or chainsaw may be easier to handle than a guided circular saw. Thick impact-absorbing surfacing tiles also do not require a special machine: a coarse-toothed wood saw blade or a rubber saw blade is suitable. A coarse tooth pattern and moderate speed keep frictional heat low, allowing fitness tiles and patio tiles made from rubber granules to be cut cleanly.
Installation of rubber tiles requires a load-bearing substrate designed to drain water. The tiles are water-permeable, so rainwater passing through them must infiltrate into the substrate or, alternatively, be discharged by a fall.
In central Europe, the suitable installation temperature is between 5 and 17 °C. Direct sunlight should be avoided, as it can cause tiles to heat up to differing degrees; throughout installation, all tiles should have an even temperature. Rain during installation does not harm the tiles, but soaked tiles must dry completely before installation.
General installation instructions must be followed, along with the requirements for the relevant product and installation system.
New rubber tiles may carry harmless release-agent residues from manufacture. Weathering washes these residues away; if required, they can be removed with water and a brush or with a pressure washer. The typical rubber smell of new tiles is harmless and reduces noticeably after a short time outdoors.
In terrace and path construction, the sub-base is the lowest layer of the pavement construction, between the formation level and the slab surfacing, while the embankment is the layer below the formation level.
A sub-base must be level, load-bearing and not susceptible to frost. It takes the loads from the surfacing and distributes them so that the ground can carry them.
Technically, an embankment is the built-up earth body below the formation level. Undisturbed natural ground lies beneath it. In everyday usage, the whole construction below a slab surfacing is often called the embankment. Here, the term is used in this wider sense.
Three groups of sub-base are distinguished. Unbound sub-bases consist of sand, gravel, chippings or crushed stone. They are laid in a loose state and compacted as far as practicable. Compaction increases their load-bearing capacity without binding the aggregate.
Grid sub-bases consist of gravel grids, also known as grass grids, gravel cells or plastic cellular grids. Their chambers are filled with chippings. Metal open-grid grating is another type of grid sub-base and can be found, for example, on balconies.
Bound sub-bases form a rigid, composite load-bearing layer. They include hydraulically bound sub-bases such as concrete, bitumen-bound sub-bases such as asphalt, existing surfacings such as concrete block paving, tiles, natural stone slabs, screed or parquet, and waterproofing layers such as roofing membranes. Under road construction standards, only concrete and asphalt are classified as sub-bases. Existing surfacings and waterproofing layers are not. All three groups are treated as sub-bases here because they all support rubber slabs.
For most rubber tiles to stay level on stone chippings or gravel in the long term, the loose material must first be stabilised with plastic honeycomb grids. These are sold under various names, including gravel grids, grass grids and honeycomb gravel grids. In each case, the cells hold the chippings in place and stop them shifting.
Chippings are generally of a similar size, with no fine material to fill the gaps between them. They cannot therefore be compacted effectively and remain prone to movement. Walk across chippings or gravel and you can feel them shift underfoot and hear them crunch. Beneath a rigid concrete slab, that movement hardly matters. Beneath a rubber tile 2 to 5 cm thick, however, hollows develop in the bed and show through on the tile surface.
First, remove the topsoil and level the ground to the required formation level. Spread a thin layer of chippings over the prepared ground and screed it carefully to a flat finish. Lay the gravel grids on top and fill the cells flush with their upper edges. Use crushed chippings rather than rounded gravel, as their angular particles interlock much better. Then lay the rubber tiles on this bed. Where the ground has poor load-bearing capacity, or where the build-up needs to withstand frost, install and compact a sub-base beneath the laying course of chippings.
Certain WARCO ranges with a flat underside are approved for installation directly on a bed of chippings, without a gravel grid. These ranges always require a sub-base of compacted crushed stone (MOT Type 1). Over this, spread a 2 to 3 cm laying course of crushed sand and chippings graded 0/5, then screed it level and compact it with a plate compactor. Unlike chippings alone, this mix contains fine sand, which allows it to firm up.
The laying course must remain within that thickness range. Below 2 cm, it cannot be screeded and compacted properly; above 3 cm, too much loose material remains beneath the patio tiles. After compaction, check the surface with a three-metre straightedge: the gap beneath it should be no more than 0.5 cm anywhere.
A permeable sub-base does not generally require a slope. In technical terms, it is a water-permeable load-bearing layer through which rainwater can infiltrate naturally into the ground.
This natural infiltration costs less than artificial drainage into the surface water sewer system, is ecologically beneficial and supports both the natural water cycle and groundwater recharge. For the system as a whole to provide effective infiltration, the surface covering must have high water permeability. Rubber tiles made from PU-bound rubber granules are particularly suitable for water-permeable systems, including patio tiles, playground tiles and tiles for many other outdoor areas. Suitable surface coverings made from rubber granules achieve a water permeability of 200 litres per hour per square metre or more.
Outdoor rubber tiles should be cleared of leaves, soil and sand regularly.
Loose dirt can be swept away with a rubber broom or rinsed off with a hose. Rain also washes much of the dust and pollen away through water-permeable tiles.
Regular maintenance reduces the work required for more thorough cleaning.
For thorough outdoor cleaning, a pressure washer is suitable. The water jet loosens dirt from the textured surface and removes more persistent residues such as dog mess or food residue.
Where clean water is not sufficient, use either a neutral cleaner suitable for rubber or a mildly acidic cleaner. A specialist rubber cleaner is not required. Biodegradable Sonett WC Cleaner Mint is particularly suitable and has a pH value of around 5 to 6.
Apply the cleaner evenly, either neat or slightly diluted. After 10 to 15 minutes, work it in with a brush, then rinse the area thoroughly with clean water.
When brushing, use moderate pressure only. Excessive pressure can loosen granules from the bonded matrix.
Strongly alkaline cleaners, abrasive products and solvent-based cleaning products are unsuitable, as they can attack the surface of the rubber tiles.